Cold extrusion sleeve

Cold extruded steel sleeve is a processing method that places a metal blank in a cold extrusion mold cavity, applies pressure to the blank through a fixed convex mold on a press at room temperature, and causes plastic deformation of the metal blank to produce the sleeve.
Surface Treatment:Natural color | Annealing treatment
material:20 # Carbon Steel
product details
来源: 最后更新时间:2025-02-12 09:12:33 人气:102276
Before carrying out the extrusion connection work on the cold extruded steel bar sleeve, it is necessary to mark the end of the steel bar (positioning mark, inspection mark). The main purpose of the positioning mark is to indicate the position of the steel bar and the sleeve. As the steel sleeve elongates after extrusion, the positioning mark enters the joint, so the inspection mark is set up to conveniently check whether the position of the steel sleeve is correct.


The construction process of cold extruded steel sleeve is as follows:
1) Check that the steel sleeve, steel bars, extrusion equipment, power supply, etc. must meet the construction requirements.
2) Mark with red paint at 100mm from the connected end of the steel bar.
3) Place a positioning mark at the end marked with red paint, and the distance between the positioning mark and the end of the steel bar is 1/2 of the length of the steel sleeve. Check the depth of steel bar insertion into the sleeve according to the positioning mark.
4) Insert the steel bars into the sleeve and use an extruder with a rated working pressure of 80 MPa and a rated extrusion pressure of 760 kN to press and connect the sleeve. Before squeezing, a qualified unit should be commissioned to calibrate the pressure of the oil gauge.
5) When operating the extruder, the pressure for squeezing the steel bars connected with diameter 25 should be controlled at 40 MPa, and the small diameter of the indentation should be between 37 mm and 39 mm. The indentation size should not be less than 50 mm, and 5 indentations should be made on each side as required. The indentation should be evenly distributed. When squeezing the next pass, due to reduced restraint, the pressure should be controlled to be 2 MPa to 4 MPa lower than the pressure of other indentation passes to prevent the diameter of the small indentation in the next pass from becoming smaller or exceeding the lower limit.
6) After the completion of the steel bar cold extrusion sleeve, a dedicated person will be sent to conduct quality inspection. When the inspection conditions are met, a qualified unit will be commissioned to conduct on-site random sampling inspection.
| List of parameters for national standard cold extruded steel sleeve | |||||
| 规格 | 长度 | 外径 | 壁厚 | 单重 | 每包数量 |
| Φ16 | 100 | 30 | 4.5 | 0.28 | 100 |
| Φ18 | 118 | 34 | 5.7 | 0.47 | 70 |
| Φ20 | 120 | 36 | 6 | 0.53 | 60 |
| Φ22 | 132 | 40 | 6.8 | 0.74 | 45 |
| Φ25 | 150 | 45 | 7.5 | 1.04 | 30 |
| Φ28 | 162 | 50 | 8 | 1.45 | 25 |
| Φ32 | 192 | 55 | 9 | 2 | 12或15 |
| Φ36 | 216 | 63 | 10 | 2.83 | 10 |
| Φ40 | 240 | 70 | 11 | 4.7 | 8 |
List of parameters for iron standard cold extruded steel sleeve | |||||
| 规格 | 长度 | 外径 | 壁厚 | 单重 | 每包数量 |
| Φ14 | 95 | 28 | 4.5 | 120 | |
| Φ16 | 110 | 30 | 4.5 | 0.28 | 100 |
| Φ18 | 125 | 34 | 5.7 | 0.47 | 70 |
| Φ20 | 130 | 36 | 6 | 0.58 | 60 |
| Φ22 | 140 | 40 | 6.8 | 0.75 | 45 |
| Φ25 | 170 | 45 | 7.5 | 1.18 | 30 |
| Φ28 | 190 | 50 | 8 | 1.58 | 25 |
| Φ32 | 200 | 55 | 9 | 2 | 15 |
| Φ36 | 220 | 63 | 10 | 3.14 | 10 |
| Φ40 | 250 | 70 | 11 | 4.37 | 8 |
If the customer does not provide a definite type and specification of the sleeve, the customer should correctly explain their type, specification, and requirements, and sign the contract under the condition of mutual understanding between the supply and demand parties。
1、The customer communicated the product type, specifications, and dimensions to our salesperson。
2、Received customer specifications and dimensions, provided sleeve quotation (price list) for the customer。
3、Specific agreement: delivery time, special requirements, and other matters。
4、After placing the order and making payment, our company will arrange shipment as soon as possible。
The characteristics of cold extrusion steel sleeve technology:
1. The construction process of cold extruded steel sleeve technology is simple and easy to master.
2. Cold extrusion steel sleeve technology is fast in construction and can save a lot of time compared to traditional welding methods.
3. Cold extruded steel sleeve technology can reduce engineering costs compared to traditional steel welding connection construction.
4. Cold extrusion steel sleeve technology is suitable for radial extrusion connection of ribbed steel bars with diameters ranging from 16 to 40 in reinforced concrete structures.